Customization: | Available |
---|---|
Material: | Zircon, Zro2 |
Refractoriness (℃): | 1580< Refractoriness< 1770 |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Item |
Testing Condition | Unit | Zirconia |
Bulk Density |
g/cm3 |
6 |
|
Flexural Strength |
N/m2 ×103 |
11 |
|
Coefficient of Linear Expansion |
20-800°C |
×10-6 /°C |
9.5 |
Bulk Density Resistance |
100°C |
Ω@Cm |
>1012 |
Bending Strength |
Mpa |
950 |
|
Thermal Conductivity |
20°C |
W/m@k |
3 |
Breaking Tenacity |
Mpa@m1/2 |
6 -8 |
|
Highest TemperatureResistance |
°C |
2300 |
|
Wear-resistance Property |
Excellent |