Customization: | Available |
---|---|
Application: | Refractory |
Purity: | 95% |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Ceramic Property Table | |||||||||
Performance | Unit | 75 Porcelain | 90 Porcelain | 95 Porcelain | 99 Porcelain | 99.7 Porcelain | Zirconia | High-Frequency Porcelain | |
Bulk Density | >3.2 | >3.4 | >3.6 | 3.7 | 3.7 | 6 | ≥2.6 | ||
Bending Strength | N/m2*103 | 1.96 | 2.25 | 2.24 | >2.24 | >2.27 | 11 | 1.37 | |
Linear Expansion Coefficient | 20-800ºC | x10-6ºC | - | 6.3-7.3 | 6.5-8 | 6.5-8 | 6.5-8 | 9.5 | ≤8 |
Dielectric Constant | 1MHz | ≤9 | 8.5-9.5 | 9-10 | 9-10.5 | 9-10.5 | - | ≤7.5 | |
10GHz | - | - | 9-10 | 9-10.5 | - | - | - | ||
Dielectric Loss | 1MHz | x10-6 | ≤10 | ≤8 | ≤4 | ≤2.5 | ≤1.5 | - | ≤8 |
10GHz | x10-6 | - | - | ≤10 | ≤6 | - | - | - | |
Specific Volume Resistance | 100ºC | Ω·Cm | >1012 | >1012 | >1013 | >1013 | >1014 | >1014 | >1012 |
Breakdown Strength | KV/mm | 20 | 15 | 15 | 15 | - | - | 20 | |
Thermal Conductivity | 20ºC | W/m·k | - | 16.8 | 25.2 | 25.2 | 29.2 | 3 | 2.9 |
Al2O3 Purity(%)
|
95
|
99.7
|
Bulk Density
|
3.6 g/cm3
|
3.9 g/cm3
|
Bending Strength
|
364
|
450
|
Expansion
|
7.6
|
8.0
|
Thermal Conductivity
|
20
|
35
|
Dielectric strength
|
11
|
12
|
Max working temperature
|
1500
|
1800
|
Water absorption
|
<0.2
|
<0.1
|